News center

Company News

Why can the same material be cleaned in the laboratory but not on site?

2026-11-18

Many customers have conducted magnetic separation tests before selection, and tested the samples in the laboratory. The iron removal effect is very ideal, and the iron content can be reduced to below the expected value. The equipment can be pulled to the site and installed, but with the same materials and parameters, the iron content of the finished product always differs. The problem often lies not in the equipment itself, but in several easily overlooked variables between laboratory conditions and production line conditions.

Laboratory samples are usually dried, and the moisture content of production line materials often exceeds the standard. Dry magnetic separation is extremely sensitive to material moisture. When conducting experiments in the laboratory, samples are usually dried to below 1%, and the magnetic separation effect is naturally good. But the materials on the production line often do not have sufficient cooling and dehumidification after coming out of the dryer, and the moisture content may fluctuate between 1.5% -2%. The extra moisture of a few tenths of a point is enough to cause the fine powder to agglomerate and adhere on the surface of the magnetic roller, shielding the magnetic field lines and reducing the iron removal efficiency from over 90% in the laboratory to below 60%. It is recommended to install an online moisture detector in front of the magnetic separator to ensure that the moisture content of the feed truly meets the standard, rather than relying on hand feel to judge that it looks dry.

Laboratory experiments use static or small batch feeding, while production lines use continuous dynamic feeding. In the laboratory, a thin layer of material is laid on the magnetic roller, and each sand particle has a chance to get close to the magnetic pole. When the feeding amount on the production line is increased, the thickness of the material layer changes from a few millimeters to more than ten millimeters or even thicker. The magnetic particles at the bottom layer are too far away from the surface of the magnetic roller, and the magnetic field force rapidly decays. The laboratory data reflects the sorting effect under ideal fabric conditions, and any slight unevenness or fluctuation in the thickness of the material layer on the production line may compromise the effect. It is recommended to install a vibrating feeder in front of the magnetic separator to stabilize the thickness of the material layer at 5-8mm, and regularly check whether the feeder is worn and causing material deviation.

Laboratory experiments are often conducted only once, while the properties of materials on the production line are constantly changing. Different mining depths, fluctuations in front-end grinding fineness, and even differences in the degree of weathering of ore surfaces during rainy and dry seasons can all lead to changes in the occurrence of magnetic impurities in materials. The samples used in the laboratory experiment may have happened to be batches with lower iron content and stronger magnetism, and the material properties have already changed when the production line runs continuously. It is recommended to take samples and send them for inspection once every quarter, and adjust the parameters of the magnetic separator in a timely manner according to the actual material properties, rather than using one set of parameters to the end.

Laboratory data is a reference for selection, not a guarantee of production line performance. When selecting equipment, sufficient margin should be left, and after production, fine adjustments should be made according to the actual material status to truly unleash the design capabilities of the magnetic separator. Encountering problems during equipment operation, welcome to contact the technical team of Shandong Heavy Industry for communication: Manager Zhang 13583776655 (same as WeChat).


Return
WhatsApp QR code