News center

Company News

Why is the iron removal effect still poor when the magnetic field of the magnetic separator is sufficient?

2026-11-19

During the installation and debugging of the equipment, a Gaussian meter was used to measure the magnetic field strength on the surface of the magnetic roller, which was 12000Gs. The data fully met the standard, and the manufacturer accepted it as qualified. The customer was also reassured. After a period of production, the iron content of the finished product remains so low that no matter how it is adjusted, it cannot be reduced below the target value. At this point, many people began to suspect that the magnetic material had demagnetized, but the retested magnetic field strength still met the standard. Where exactly is the problem?

Gauss measures the surface of the magnetic roller, but the material is "sensing" the magnetic field through a layer of material. The magnetic force decays rapidly with distance, and at a distance of 5mm from the surface of the magnetic roller, the magnetic field strength may only be 30% of the surface, while at a distance of 10mm, it may be less than 10%. The thickness of the material layer on the production line is usually 5-10mm, and the bottom material is far away from the surface of the magnetic roller. The actual felt magnetic field force is much lower than the surface measurement value. During laboratory experiments, the material layer is only thin, and each sand particle is attached to a magnetic roller, resulting in a naturally good effect. When the material layer on the production line is thick, the weak magnetic particles at the bottom cannot be absorbed and are directly discharged with the sand. The solution is not to replace the magnetic material, but to reduce the thickness of the material layer by installing a vibrating cloth feeder to stabilize the material layer within 5mm, while appropriately reducing the feeding speed to allow each sand particle to have a chance to approach the surface of the magnetic roller.

The surface of the magnetic roller appears clean, but in reality, there is a layer of "fouling film" that is invisible to the naked eye. Quartz sand generates a large amount of fine dust during the crushing and grinding process, which gradually deposits on the surface of the magnetic roller, forming a thin powder film. The powder film is not thick and may not be felt by hand, but it is separated between the magnetic roller and the material, which is equivalent to increasing the thickness of the material layer and further weakening the magnetic field force. Even more discreetly, some mineral sources contain trace amounts of oily substances, forming an oil film on the surface of the magnetic roller. The fine powder is stuck by the oil and accumulates thicker, making it impossible to remove with a brush during cleaning. It is recommended to wipe the surface of the magnetic roller with anhydrous ethanol or cleaning agent every shift, rather than just using a brush for dry sweeping. When oil gloss or sticky texture is found on the surface of the magnetic roller, it indicates that an oil film has formed and needs to be thoroughly cleaned.

The ratio of the magnetic roller speed to the feeding speed determines the actual residence time of the material in the magnetic field zone. Many operators only focus on whether the magnetic roller speed is normal, but ignore whether the feeding speed matches. When the speed of the magnetic roller remains constant and the feeding speed increases, the residence time of the material on the magnetic roller is shortened, and the magnetic particles slide over before they can be adsorbed. When the feeding speed remains constant and the magnetic roller speed increases, the material distribution on the magnetic roller becomes thinner. However, as the speed increases, it also affects the adsorption effect. The correct approach is to adjust the magnetic roller speed and feeding speed as a whole, and maintain the material's residence time in the magnetic field zone not less than 1.5 seconds. When making actual adjustments, first fix the feeding speed and gradually adjust the magnetic roller speed. After each adjustment, take a sample to test the iron content and find the best matching point.

Meeting the standard for magnetic field strength is only a necessary condition, not a sufficient condition. The actual magnetic field force felt by the material is the key to determining the effectiveness of iron removal. Encountering problems during equipment operation, welcome to contact the technical team of Shandong Heavy Industry for communication: Manager Zhang 13583776655 (same as WeChat).


Return
WhatsApp QR code